Copper Jewelry Lost Wax Casting Powder, 100g Powder/38–40mL Water Reference, 750°C Maximum Burnout

Let’s define your requirement

Send a product link, drawing or short brief. We’ll work through the details with you.

  1. Confirm the specificationGrade or model, size and intended use.
  2. Define your orderQuantity, finish or configuration, and samples.
  3. Agree the quotation scopeIncluded work, key checks and delivery needs.
View the enquiry checklist
Product description
  • Color
    Copper , Silver , Gold
  • Warranty
    1 Year
    After-sale Service
    Online Technical Support, Onsite Inspection, Other
  • fluidity
    15-18CM, more than 18cm
    Project Solution Capability
    Others
  • Application
    Diy, Workshop
    Design Style
    Modern
  • surface smoothness
    Smooth
    air bubbles
    minimal air bubbles, no air bubbles
  • flexural strength mpa
    Other
  • Powder / Water Ratio
    100g powder : 38-40ml wate
    Expansion Rate
    ≤0.08%
  • Initial Setting Time
    10 - 12 minutes
    Max. Burnout Temperature
    750°C (1382°F)
  • Working Time
    8 - 10 minutes

Lost wax casting powder is offered for copper-jewelry DIY and workshop requests. The powder/water mixing reference is 100 g powder to 38–40 mL water. Choose the actual gold, silver or copper selection label and confirm its color/formulation or intended-alloy role for the jewelry process.

Working interval and initial setting

Working time is 8–10 minutes, while initial setting time is 10–12 minutes. Agree the selected formulation's preparation and measurement conditions for those separate intervals. Define the actual mixing and investment procedure against the jewelry pattern and accepted working sequence.

Maximum burnout and expansion limit

Maximum burnout temperature is 750°C (1382°F), with expansion no more than 0.08%. Confirm the selected powder's actual test and operating conditions. Obtain the complete burnout instructions for the investment process, keeping the maximum-temperature reference separate from the required schedule and any molten-metal temperature.

Fluidity and smooth-surface acceptance

Fluidity directions are 15–18 cm and more than 18 cm. Confirm which result applies to the chosen formulation and how it is measured. Smooth surface and minimal/no-bubble conditions are acceptance directions to agree under the actual preparation process. Define the accepted surface and bubble level for the particular jewelry job.

Option role and offered support

Match the selected powder option to the actual alloy and investment requirements after its designation is clarified. Online technical support and onsite inspection are offered. A one-year warranty is available, with its actual powder/service coverage to agree. Confirm the formulation, operating instructions and required acceptance with that support scope before choosing the powder.